Dow VORANOL™ CP 755 Polyol

Category Polymer , Thermoset
Manufacturer Dow Chemical
Trade Name VORANOL™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow VORANOL™ CP 755 Polyol.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
VORANOL™ CP 755 polyol is a glycerine propoxylated polyether triol.Information provided by Dow
Physical Properties Metric English Comments
Specific Gravity 1.07 g/cc
1.07 g/cc
pH 4.5 - 6.5
4.5 - 6.5
(1 Water / 10 Methanol); DOWM 101495-TE94A
Viscosity Measure 225 - 260 cSt

@Temperature 25.0 °C
225 - 260 cSt

@Temperature 77.0 °F
ASTM D445-94
Molecular Weight 700 g/mol
700 g/mol
Maximum Moisture Content 0.050
0.050
wt% water; ASTM E203-96
ASTM Color <= 50
<= 50
APHA; ASTM D4890-93
Thermal Properties Metric English Comments
Flash Point 180 - 214 °C
356 - 417 °F
Pensky Martens closed cup
Chemical Properties Metric English Comments
Total Acid Number 0.10
0.10
[mg KOH/g]; DOWM 100387-TE95A
Ionic Impurities - Na (Sodium) <= 10 ppm
<= 10 ppm
AOD-S
Ionic Impurities - K (Potassium) <= 10 ppm
<= 10 ppm
AOD-S
Descriptive Properties Value Comments
Hydroxyl Number mg KOH/g 225 - 250
ASTM D4274-94d