Dow VORANOL™ RA 800 Polyol

Category Polymer , Thermoset
Manufacturer Dow Chemical
Trade Name VORANOL™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow VORANOL™ RA 800 Polyol.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
VORANOL™ RA 800 polyol is a highly reactive amine initiated polyether polyol, specially developed for the production of rigid polyurethane foams and designed for blending with other polyols.Information provided by Dow
Physical Properties Metric English Comments
Specific Gravity 1.07 g/cc
1.07 g/cc
Viscosity Measure 3550 cSt

@Temperature 37.8 °C
3550 cSt

@Temperature 100 °F
ASTM D445-94
15000 - 19000 cSt

@Temperature 25.0 °C
15000 - 19000 cSt

@Temperature 77.0 °F
ASTM D445-94
Maximum Moisture Content 0.10
0.10
wt% water; ASTM E203-96
Thermal Properties Metric English Comments
Flash Point 205 °C
401 °F
Optical Properties Metric English Comments
Gardner Color Number <= 5.0
<= 5.0
ASTM D4890-93
Descriptive Properties Value Comments
Basicity meq/g, min 3.4 - 3.7
DOWM 101485-TE94A
Hydroxyl Number mg KOH/g 780 - 820
ASTM D4274-94d