Material Notes:
XU 66129.00 Developmental Monolayer Adhesive Film is a heat-activated, thermally stable adhesive film capable of bonding to urethane foam-backed fabrics, paper, fiberglass, non-wovens, and rigid urethanes.Information provided by Dow
Physical Properties Metric English Comments
Thickness 50.8 microns
2.00 mil
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 610 %
610 %
ASTM D882
Film Elongation at Break, TD 560 %
560 %
ASTM D882
Secant Modulus, MD 0.338 GPa
49.0 ksi
2% Secant; ASTM D882
Secant Modulus, TD 0.462 GPa
67.0 ksi
2% Secant; ASTM D882
Elmendorf Tear Strength, MD 0.787 g/micron
20.0 g/mil
ASTM D882
Elmendorf Tear Strength, TD 3.15 g/micron
80.0 g/mil
ASTM D882
Film Tensile Strength at Break, MD 23.4 MPa
3400 psi
ASTM D882
Film Tensile Strength at Break, TD 17.9 MPa
2600 psi
ASTM D882