Material Notes:
Appeel® 20D784 is a modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a broad temperature range to a number of container materials including PP, PS, and some PVC types. Appeel® 20D784 is available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene resins. APPEEL® 20D784 Lidding Sealant Resin complies with Food and Drug Administration Regulation 21 CFR 177.1340 - - Ethylene-methyl acrylate copolymer resins, subject to the limitations and requirements therein. This Regulation describes polymers that may be used in contact with food, subject to the finished food-contact article meeting the extractive limitations under the intended conditions of use, as shown in paragraph (b) of the Regulation.
Physical Properties Metric English Comments
Density 0.930 g/cc
0.0336 lb/in³
ASTM D792, ISO 1183
Melt Flow 9.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
9.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238, ISO 1133
Thermal Properties Metric English Comments
Melting Point 98.0 °C
208 °F
ASTM D3417, ISO 3146
Vicat Softening Point 60.0 °C
140 °F
ASTM D1525, ISO 306
Processing Properties Metric English Comments
Processing Temperature <= 300 °C
<= 572 °F
Feed Temperature 140 °C
284 °F
Blown Film Coextrusion
160 °C
320 °F
Extrusion Coating
Zone 2 150 °C
302 °F
Blown Film Coextrusion
210 °C
410 °F
Extrusion Coating
Zone 3 160 °C
320 °F
Blown Film Coextrusion
235 °C
455 °F
Extrusion Coating
Zone 4 180 °C
356 °F
Blown Film Coextrusion
260 °C
500 °F
Extrusion Coating
Zone 5 180 °C
356 °F
Blown Film Coextrusion
285 °C
545 °F
Extrusion Coating
Adapter Temperature 180 °C
356 °F
Blown Film Coextrusion
285 °C
545 °F
Extrusion Coating
Die Temperature 170 °C
338 °F
Blown Film Coextrusion
285 °C
545 °F
Extrusion Coating
Melt Temperature 160 - 185 °C
320 - 365 °F
Blown Film Coextrusion
235 - 285 °C
455 - 545 °F
Extrusion Coating
Copyright © lookpolymers.com All Rights Reserved