Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont™ Bynel® 22E757 Modified Ethylene Acrylate

Category Polymer , Thermoplastic , Adhesives, Sealants, and Coatings
Manufacturer DuPont
Trade Name Bynel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont™ Bynel® 22E757 Modified Ethylene Acrylate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BYNEL® Series 2200 resins are modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene (PE) resins. BYNEL 22E757 resin conforms with the Code of Federal Regulations, Title 21, Paragraph 177.1340, covering use in contact with all types of food, subject to meeting the migration limits specified in the regulation.
Physical Properties Metric English Comments
Density 0.940 g/cc
0.0340 lb/in³
ASTM D792, ISO 1183
Melt Flow 8.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238, ISO 1133
Thermal Properties Metric English Comments
Melting Point 92.0 °C
198 °F
ASTM D3418, ISO 3146
Vicat Softening Point 54.0 °C
129 °F
ASTM D1525, ISO 306
Processing Properties Metric English Comments
Processing Temperature <= 310 °C
<= 590 °F
Feed Temperature 160 °C
320 °F
Extrusion Coating
Zone 2 210 °C
410 °F
Extrusion Coating
Zone 3 260 °C
500 °F
Extrusion Coating
Zone 4 285 °C
545 °F
Extrusion Coating
Zone 5 285 °C
545 °F
Extrusion Coating
Adapter Temperature 285 °C
545 °F
Extrusion Coating
Die Temperature 285 °C
545 °F
Extrusion Coating
Melt Temperature 210 - 235 °C
410 - 455 °F
CoExtrusion with EVOH Processing
<= 310 °C
<= 590 °F
CoExtrusion with Nylon Processing
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved