DuPont™ Clysar® VHP Polyolefin Shrink Packaging Film, 50 Gauge  (discontinued **)

Category Polymer , Film , Thermoplastic , Polyolefin , Polyolefin, Film Grade , Polyolefin, Film Grade (Polyolefin)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont™ Clysar® VHP Polyolefin Shrink Packaging Film, 50 Gauge  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by DuPont Packaging Polymers.DuPont Clysar® VHP is a thin gauge, clear, biaxially oriented, heat shrinkable polyolefin film. It provides strong seals and excellent optics under a wide range of operating conditions.DuPont Clysar® VHP is designed for the packaging of lightweight, low-abuse products. It combines excellent optics and seal strength with the economics of high yield, reduced changeover and downtime, and greater use of storage space.
Physical Properties Metric English Comments
Moisture Vapor Transmission 0.440 cc-mm/m²-24hr-atm
1.12 cc-mil/100 in²-24hr-atm
ASTM 1249
Oxygen Transmission 236 cc-mm/m²-24hr-atm
599 cc-mil/100 in²-24hr-atm
or 14100 cc/m²-24hr-atm for the 50 gauge film. ASTM D3985
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 115 %
115 %
Average; ASTM D882
Secant Modulus 0.410 GPa
59.5 ksi
Stiffness Modulus; ASTM D882
Impact Test 1.13 J
0.833 ft-lb
Spencer Impact ASTM D3420
Coefficient of Friction, Dynamic 0.30
0.30
ASTM D1894
Elmendorf Tear Strength MD 15 g
15 g
Orientation not specified; ASTM D1922
Film Tensile Strength at Break, MD 103 MPa
14900 psi
ASTM D882
Optical Properties Metric English Comments
Haze 15 %
15 %
ASTM D1003
Gloss 145 %
145 %
at 20°; ASTM D2457