Material Notes:
Elvaloy® AC 2618 is a copolymer of ethylene and ethyl acrylate. It is available in pellet form for use in conventional extrusion equipment designed to process polyethylene type resins. Elvaloy® AC 2618 resin complies with the U. S. Food and Drug Administration regulation 21 CFR177.1320; Ethylene Ethyl Acrylate copolymers, for use in contact with food, except for holding food during cooking. These EEA resins must be blended with olefin polymers complying with 21 CFR 177.1520 in such proportions that the ethyl acrylate content of the blend does not exceed 8 percent by weight. Migration limits must also be complied as specified in paragraph (c)(2).
Physical Properties Metric English Comments
Density 0.930 g/cc
0.0336 lb/in³
ASTM D792, ISO 1183
Melt Flow 6.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
6.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238, ISO 1133
Thermal Properties Metric English Comments
Melting Point 95.0 °C
203 °F
ASTM D3418, ISO 3146
Vicat Softening Point 56.0 °C
133 °F
ASTM D1525, ISO 306
Processing Properties Metric English Comments
Processing Temperature <= 310 °C
<= 590 °F
Feed Temperature 185 °C
365 °F
Extrusion Coating
Zone 2 235 °C
455 °F
Extrusion Coating
Zone 3 260 °C
500 °F
Extrusion Coating
Zone 4 285 °C
545 °F
Extrusion Coating
Zone 5 285 °C
545 °F
Extrusion Coating
Adapter Temperature 285 °C
545 °F
Extrusion Coating
Die Temperature 285 °C
545 °F
Extrusion Coating
Melt Temperature 235 - 310 °C
455 - 590 °F
Extrusion Coating