Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Elvax® 3129 Ethylene-Vinyl Acetate Copolymer Resin for Blown Film  (discontinued **)

Category Polymer , Film , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate Copolymer (EVA), Film Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Elvax® 3129 Ethylene-Vinyl Acetate Copolymer Resin for Blown Film  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
10 wt% Vinyl Acetate.General Elvax® information: Elvax® packaging grade resins include low seal temperatures for use in coextrusions or for packaging temperature sensitive materials, excellent drawability for easy processing, good flex-crack resistance for liquid packaging, high toughness, low shrink for water bath applications, and excellent optical properties. It adheres to many materials. It is commonly used as a tie layer in certain coextrusions with dissimilar surfaces.Information provided by DuPont Packaging Polymers.
Physical Properties Metric English Comments
Density 0.930 g/cc
0.0336 lb/in³
ASTM D792
Melt Flow 0.35 g/10 min
0.35 g/10 min
Condition not noted.; ASTM D1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 620 %
620 %
MD-TD Average; ASTM D882
Film Elongation at Break, TD 620 %
620 %
MD-TD Average; ASTM D882
Impact 36.9
36.9
J/mm Spencer Impact; Average of MD and TD; ASTM D3420
Elmendorf Tear Strength, MD 1.77 g/micron
45.0 g/mil
Average of MD and TD; ASTM D1922
Film Tensile Strength at Break, MD 33.7 MPa
4890 psi
MD-TD Average; ASTM D882
Thermal Properties Metric English Comments
Melting Point 82.0 °C
180 °F
Freezing Point via DSC/ASTM D3418
100 °C
212 °F
Upon Melting via DSC/ASTM D3418
Vicat Softening Point 87.0 °C
189 °F
ASTM D1525
Optical Properties Metric English Comments
Haze 2.0 %
2.0 %
ASTM D1003
Gloss 121 %
121 %
20°; ASTM D2457