Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Elvax® 3174 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Cast Film  (discontinued **)

Category Polymer , Film , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Elvax® 3174 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Cast Film  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
18 wt% Vinyl Acetate.Elvax® 3174 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins.Additives: Antioxidant.Applications: Elvax® 3174 is designed to provide a low temperature heat seal to itself or many other materials commonly used in flexible packaging applications. The melt properties of this resin allow it to be processed on cast film equipment over a wide range of line speeds and film thicknesses. It can also be coextruded with a variety of other polymers. Elvax® 3174 is typically used as a low-temperature seal layer in coextruded films. Information provided by DuPont Packaging Polymers.
Physical Properties Metric English Comments
Density 0.940 g/cc
0.0340 lb/in³
ASTM D792
Melt Flow 8.0 g/10 min
8.0 g/10 min
Condition not noted.; ASTM D1238
Thermal Properties Metric English Comments
Melting Point 65.0 °C
149 °F
Freezing Point via DSC/ASTM D3418
86.0 °C
187 °F
Upon Melting via DSC/ASTM D3418
Vicat Softening Point 61.0 °C
142 °F
ASTM D1525
Processing Properties Metric English Comments
Melt Temperature 150 - 205 °C
302 - 401 °F
cast film extrusion.
Users viewing this material also viewed the following: