DuPont Elvax® 40L-08 Strippable Semiconductive Insulation Shield Formulation  (discontinued **)

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Elvax® 40L-08 Strippable Semiconductive Insulation Shield Formulation  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Elvax® 40L-08 strippable semiconductive insulation shield.Information provided by DuPont.
Mechanical Properties Metric English Comments
Tensile Strength at Break 10.89 MPa
1579 psi
After 7 days/121°C air oven, ASTM D573
12.1 MPa
1750 psi
ASTM D412
Elongation at Break 210 %
210 %
After 7 days/121°C air oven; ASTM D573
250 %
250 %
ASTM D412
Tear Strength 8.50 kN/m
48.5 pli
ASTM D470
Electrical Properties Metric English Comments
Electrical Resistivity 116 ohm-cm

@Temperature 130 °C
116 ohm-cm

@Temperature 266 °F
ASTM D991-82
174 ohm-cm

@Temperature 23.0 °C
174 ohm-cm

@Temperature 73.4 °F
ASTM D991-82
179 ohm-cm

@Temperature 90.0 °C
179 ohm-cm

@Temperature 194 °F
ASTM D991-82
Descriptive Properties Value Comments
Antioxidant 1.5 phr
Conductive Black 50 phr
Dicumyl Peroxide 2.5 phr
Elvax® 40L-08 100 phr
Stearic Acid 1 phr
Triallyl Cyanurate 1 phr