DuPont Elvax® 4260 Ethylene Vinyl Acetate  (discontinued **)

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Elvax® 4260 Ethylene Vinyl Acetate  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DuPont™ Elvax® 4260 is an ethylene-vinyl acetate / acid terpolymer resin for use in industrial applications. Applications:Elvax® 4260 resins can be used for the following applications: adhesives, sealants, and wax blends.Information provided by DuPont™
Physical Properties Metric English Comments
Density 0.955 g/cc
0.0345 lb/in³
ASTM D1505
Vinyl Acetate Content 28 %
28 %
Melt Flow 6.0 g/10 min
6.0 g/10 min
modified; ASTM D1238, ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
ASTM D2240-ISO 868
Tensile Strength at Break 18.6 MPa
2700 psi
ASTM D1708
Elongation at Break 1000 %
1000 %
ASTM D1708
Tensile Modulus 0.0103 GPa
1.50 ksi
ASTM D1708
Thermal Properties Metric English Comments
Ring & Ball Softening Point 158 °C
316 °F
ASTM E28
Descriptive Properties Value Comments
Cloud Point in Paraffin Wax, °C 99
10% Elvax® in fully refined paraffin wax, 146 AMP. Incompatible at temperatures up to 177°C.