DuPont™ Kevlar® 149 Fiber, diam. 12 µm

Category Other Engineering Material , Composite Fibers , Polymer , Thermoset , Aramid
Manufacturer DuPont
Trade Name Kevlar®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont™ Kevlar® 149 Fiber, diam. 12 µm.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: armor, belts, hoses, composite structures, cable sheathing, gaskets, brake pads, clutch linings, friction pads, slot insulation, phase barrier insulation, interturn insulation.KEVLAR® is a DuPont registered trademark.
Physical Properties Metric English Comments
Density 1.47 g/cc
0.0531 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 3450 MPa
500000 psi
Modulus of Elasticity 179 GPa
26000 ksi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 425 °C
797 °F
Decomposition Temperature 500 °C
932 °F