Category Polymer , Thermoplastic , Nylon , Nylon, Aromatic
Manufacturer DuPont
Trade Name Nomex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont™ Nomex® Type 993, 60 mil Nominal Thickness Medium-Density Aromatic Nylon Pressboard.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Type 993 is a medium-density pressboard which offers a balance of rigidity and conformability along with outstanding saturability and excellent properties in air and oil. Typical applications include 3-dimensional parts such as V-rings, angle rings and spools, as well as barrier, gap spacers and core tubes.Information provided by DuPont
Physical Properties Metric English Comments
Density 0.730 g/cc
0.0264 lb/in³
Calculated number using basis weight and thickness
Thickness 1500 microns
59.1 mil
ASTM D374, method D, using 17 N/cm²
Linear Mold Shrinkage 0.0070 cm/cm

@Temperature 105 °C
0.0070 in/in

@Temperature 221 °F
ASTM D3392
0.015 cm/cm

@Temperature 240 °C
0.015 in/in

@Temperature 464 °F
ASTM D3392
Linear Mold Shrinkage, Transverse 0.010 cm/cm

@Temperature 105 °C
0.010 in/in

@Temperature 221 °F
ASTM D3392
0.016 cm/cm

@Temperature 240 °C
0.016 in/in

@Temperature 464 °F
ASTM D3392
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 40.0 MPa
5800 psi
ASTM D828
Film Tensile Strength at Yield, TD 33.1 MPa
4800 psi
ASTM D828
Film Elongation at Yield, MD 11.2 %
11.2 %
ASTM D828
Film Elongation at Yield, TD 12.9 %
12.9 %
ASTM D828
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+17 ohm-cm

@Temperature 130 °C
1.00e+17 ohm-cm

@Temperature 266 °F
in oil; ASTM D257
1.00e+18 ohm-cm

@Temperature 90.0 °C
1.00e+18 ohm-cm

@Temperature 194 °F
in oil; ASTM D257
Dielectric Constant 3.2

@Frequency 60.0 Hz,
Temperature 25.0 °C
3.2

@Frequency 60.0 Hz,
Temperature 77.0 °F
in oil; ASTM D150
3.2

@Frequency 60.0 Hz,
Temperature 90.0 °C
3.2

@Frequency 60.0 Hz,
Temperature 194 °F
in oil; ASTM D150
3.3

@Frequency 60.0 Hz,
Temperature 130 °C
3.3

@Frequency 60.0 Hz,
Temperature 266 °F
in oil; ASTM D150
Dielectric Strength 22.0 kV/mm
559 kV/in
AC rapid rise in air; ASTM D149
34.0 kV/mm
864 kV/in
AC rapid rise in oil; ASTM D149
73.0 kV/mm
1850 kV/in
Full wave impulse in oil; ASTM D3426
Dissipation Factor 0.0050

@Frequency 60.0 Hz,
Temperature 25.0 °C
0.0050

@Frequency 60.0 Hz,
Temperature 77.0 °F
in oil; ASTM D150
0.0050

@Frequency 60.0 Hz,
Temperature 90.0 °C
0.0050

@Frequency 60.0 Hz,
Temperature 194 °F
in oil; ASTM D150
0.0070

@Frequency 60.0 Hz,
Temperature 130 °C
0.0070

@Frequency 60.0 Hz,
Temperature 266 °F
in oil; ASTM D150
Descriptive Properties Value Comments
Basis Weight (g/m²) ASTM D3392