DuPont Nucrel® 0609HSA Ethylene-Methacrylic Acid Copolymer Resin for Film and Extrusion Coating/Laminating

Category Polymer , Film , Thermoplastic , Ethylene Methyl Acrylate , Ethylene-Methyl Acrylate Copolymer, Film Grade
Manufacturer DuPont Packaging and Industrial Polymers
Trade Name Nucrel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Nucrel® 0609HSA Ethylene-Methacrylic Acid Copolymer Resin for Film and Extrusion Coating/Laminating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
6.5 wt% Methacrylic Acid.Nucrel® 0609HSA is an ethylene-methacrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and extrusion laminating equipment designed to process polyethylene resins. This resin may also be used in conventional blown and cast film extrusion and coextrusion equipment.Features & Benefits: Excellent adhesion to unprimed foil, paper and metallized film provides better substrate protection, improved structure reliability, and barrier integrity. This product provides very good but lower adhesion to polyethylene than acid copolymers with 4% or less methacrylic acid content (e.g., Nucrel® 0407 and Nucrel® 0411HS). High speed operation on packaging machinery is enhanced by low seal initiation temperature compared to LDPE Excellent hot tack, sealability through contamination, and heat seal strength provides strong, reliable heat seals Contains anti-oxidant.Typical Applications: Foil-containing pouches and sachets; Aseptic and hot-fill liquid cartons; Lidding and snack structures; Other foil, metallized film, or paper coatings as a heat seal or tie layer.Information provided by DuPont Packaging Polymers.
Physical Properties Metric English Comments
Melt Flow 9.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
9.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Thermal Properties Metric English Comments
Melting Point 83.0 °C
181 °F
Freezing Point via DSC/ASTM D3418
104 °C
219 °F
Upon Melting via DSC/ASTM D3418
Vicat Softening Point 88.0 °C
190 °F
ASTM D1525
Processing Properties Metric English Comments
Nozzle Temperature 300 °C
572 °F
Typical Die Temp. for Extrusion Coating
Melt Temperature 260 - 315 °C
500 - 599 °F
flat die equipment