DuPont Nucrel® 0903HC Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film

Category Polymer , Film , Thermoplastic , Ethylene Methyl Acrylate , Ethylene-Methyl Acrylate Copolymer, Film Grade
Manufacturer DuPont Packaging and Industrial Polymers
Trade Name Nucrel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Nucrel® 0903HC Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
9 wt% Methacrylic Acid.Nucrel® 0903HC (High-Clarity) is an ethylene-methacrylic acid copolymer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins.Features/Benefits vs. Nucrel® 0903: Better film optics provide better package appearance and product visibility.Typical Applications: Meat, poultry, seafood, and cheese packaging; Cereal liners; Medical/pharmaceutical packaging; Powdered/granular food and non-food pouches; Carded display/skin packaging films; Edible oil, motor oil, and other liquid product pouches; Snack structures; Coextrusions with nylon or in other film structures as a heat seal or tie layer.Information provided by DuPont Packaging Polymers.
Physical Properties Metric English Comments
Melt Flow 2.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Seal Strength 2300 g/25 mm
2300 g/in
seal bar 140°C.
Hot Tack Strength 1800 g/25 mm
1800 g/in
seal bar 105°C; Packforsk method.
Thermal Properties Metric English Comments
Melting Point 84.0 °C
183 °F
Freezing Point via DSC/ASTM D3418
102 °C
216 °F
Upon Melting via DSC/ASTM D3418
Vicat Softening Point 81.0 °C
178 °F
ASTM D1525
Processing Properties Metric English Comments
Nozzle Temperature 191 °C
376 °F
Typical Die Temp.
Melt Temperature 190 - 218 °C
374 - 424 °F
blown film equipment