Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Nucrel® 0910HS Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating/Laminating

Category Polymer , Thermoplastic , Ethylene Methyl Acrylate , Ethylene-Methyl Acrylate Copolymer, Coating Grade
Manufacturer DuPont Packaging and Industrial Polymers
Trade Name Nucrel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Nucrel® 0910HS Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating/Laminating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
8.7 wt% Methacrylic Acid.Nucrel® 0910HS (High-Stability) is an ethylene-methacrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating and extrusion laminating equipment designed to process polyethylene resins. Formerly Nucrel® RX8388-1.Features/Benefits vs. Nucrel® 0910: Higher drawability for thinner coatings and/or higher extrusion speeds results in reduced material and/or operating costs. Higher oxidation resistance to prevent off-taste and off-odor formation for fewer taste/odor complaints. Higher thermal stability for easier extrudability and purging, improved extrusion web stability, and reduced gel formation.Typical Applications: Foil-containing shampoo, toothpaste, towelette, condiment and miscellaneous non-food pouches and sachets; Snack structures; Toothpaste tubes ; Cable shield wrap; Aseptic and hot-fill liquid cartons; Other foil, metallized film, or paper coatings as a heat seal or tie layer.Information provided by DuPont Packaging Polymers.
Physical Properties Metric English Comments
Density 0.930 g/cc
0.0336 lb/in³
ASTM D792
Melt Flow 10 g/10 min

@Load 2.16 kg,
Temperature 190 °C
10 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Seal Strength 1500 g/25 mm
1500 g/in
seal bar 125°C.
Hot Tack Strength 1000 g/25 mm
1000 g/in
seal bar 110°C; Packforsk method.
Thermal Properties Metric English Comments
Melting Point 84.0 °C
183 °F
Freezing Point via DSC/ASTM D3418
103 °C
217 °F
Upon Melting via DSC/ASTM D3418
Vicat Softening Point 86.0 °C
187 °F
ASTM D1525
Processing Properties Metric English Comments
Nozzle Temperature 290 °C
554 °F
Typical Die Temp.
Melt Temperature 260 - 305 °C
500 - 581 °F
Users viewing this material also viewed the following: