DuPont Nucrel® 1214 Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating/Laminating  (discontinued

Category Polymer , Thermoplastic , Ethylene Methyl Acrylate , Ethylene-Methyl Acrylate Copolymer, Coating Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Nucrel® 1214 Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating/Laminating  (discontinued.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
12 wt% Methacrylic Acid.Nucrel® 1214 is an ethylene-methacrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and extrusion laminating equipment designed to process polyethylene resins.Features/Benefits vs. Nucrel® 1207: Higher melt flow index provides easier extrusion, higher extrusion rates, and higher flow during heat sealing. The result is fewer leakers.Typical Applications: Foil-containing shampoo, toothpaste, towelette, condiment and miscellaneous non-food pouches and sachets. Medical/pharmaceutical packaging. Snack structures. Other foil, metallized film, or paper coatings as a heat seal or tie layer.Information provided by DuPont Packaging Polymers.
Physical Properties Metric English Comments
Density 0.940 g/cc
0.0340 lb/in³
ASTM D792
Melt Flow 13.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
13.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hot Tack Strength 1100 g/25 mm
1100 g/in
seal bar 100°C; Packforsk method.
Thermal Properties Metric English Comments
Melting Point 71.0 °C
160 °F
Freezing Point via DSC/ASTM D3418
97.0 °C
207 °F
Upon Melting via DSC/ASTM D3418
Vicat Softening Point 75.0 °C
167 °F
ASTM D1525
Processing Properties Metric English Comments
Nozzle Temperature 230 °C
446 °F
Typical Die Temp.
Melt Temperature 220 - 260 °C
428 - 500 °F