Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Nucrel® 1302 Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film  (discontinued **)

Category Polymer , Film , Thermoplastic , Ethylene Methyl Acrylate , Ethylene-Methyl Acrylate Copolymer, Film Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Nucrel® 1302 Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
13 wt% Methacrylic Acid.Nucrel® 1302 is an ethylene-methacrylic acid copolymer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins.Features & Benefits: Excellent adhesion to aluminum foil. Good adhesion to low-density polyethylene.Typical Applications: Cable shield wrap. Blown film applications requiring functionality of higher acid comonomer content.Processing Nucrel® 1302 is normally processed at melt temperatures ranging from 175-200°C (347-392°F) in blown film equipment. Actual processing temperatures will usually be determined by either the specific equipment or one of the other polymers in a coextrusion. Nucrel® 1302 can also be used in cast extrusions and coextrusions.Information provided by DuPont Packaging Polymers.
Physical Properties Metric English Comments
Density 0.940 g/cc
0.0340 lb/in³
ASTM D792
Melt Flow 1.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Thermal Properties Metric English Comments
Melting Point 79.0 °C
174 °F
Freezing Point via DSC/ASTM D3418
96.0 °C
205 °F
Upon Melting via DSC/ASTM D3418
Processing Properties Metric English Comments
Nozzle Temperature 180 °C
356 °F
Typical Die Temp.
Melt Temperature 175 - 200 °C
347 - 392 °F