Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Performance Polymers Crastin® 6134 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer DuPont Performance Polymers
Trade Name Crastin®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Crastin® 6134 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Unreinforced Medium Viscosity Polybutylene Terephthalate Crastin 6134 NC010 is an unreinforced medium viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.30 g/cc
0.0470 lb/in³
ISO 1183
Melt Flow 33.5 g/10 min

@Load 2.16 kg,
Temperature 250 °C
33.5 g/10 min

@Load 4.76 lb,
Temperature 482 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 59.0 MPa
8560 psi
ISO 527-1/-2
Elongation at Break 45 %
45 %
Nominal; ISO 527-1/-2
Elongation at Yield 4.0 %
4.0 %
ISO 527-1/-2
Tensile Modulus 2.60 GPa
377 ksi
ISO 527-1/-2
Flexural Strength 85.0 MPa
12300 psi
ISO 178
Izod Impact, Notched (ISO) 3.50 kJ/m²
1.67 ft-lb/in²
ISO 180/1A
Charpy Impact, Notched 0.400 J/cm²
1.90 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 225 °C
437 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 115 °C
239 °F
ISO 75-1/-2
180 °C
356 °F
annealed; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C
122 °F
ISO 75-1/-2
60.0 °C
140 °F
annealed; ISO 75-1/-2
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
IEC 60695-11-10
Oxygen Index 22 %
22 %
ISO 4589-1/-2
Descriptive Properties Value Comments
Delivery Form Pellets
Part Marking Code >PBT<
ISO 11469
Processing Casting
Coatable
Film Extrusion
Injection Moulding
Other Extrusion
Profile Extrusion
Sheet Extrusion
Regional Availability Europe
Near East/Africa
Resin Identification PBT
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved