Material Notes:
Crastin® SC164 NC010 is an unreinforced, low viscosity polybutylene terephthalate resin for injection molding. It has been developed for consideration into applications such as parts for the healthcare industry.Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.31 g/cc
0.0473 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Yield 58.0 MPa

@Temperature 23.0 °C
8410 psi

@Temperature 73.4 °F
ISO 527
Elongation at Yield 6.0 %

@Temperature 23.0 °C
6.0 %

@Temperature 73.4 °F
ISO 527
Tensile Modulus 2.60 GPa

@Temperature 23.0 °C
377 ksi

@Temperature 73.4 °F
ISO 527
Charpy Impact, Notched 0.400 J/cm²

@Temperature 23.0 °C
1.90 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 225 °C
437 °F
10°C/min; ISO 11357-1/-3
Processing Properties Metric English Comments
Moisture Content <= 0.040 %
<= 0.040 %
Descriptive Properties Value Comments
Appearance Natural Color
Forms Pellets
Generic Polybutylene Terephthalate (PBT)
Material Status Preliminary Data
Part Marking Code >PBT<
ISO 11469
Processing Method Injection Molding
Product Category Healthcare Resins
Unreinforced Resins
Region Available - Global Yes
Resin Identification PBT
ISO 1043
Uses Medical Applications
Users viewing this material also viewed the following: