DuPont Performance Polymers Hytrel® HTR8785 BK482 Polyester Elastomer TPC-ET  (Unverified Data**)

Category Polymer , Thermoplastic , Polyester, TP , Polyester Thermoplastic Elastomer
Manufacturer DuPont Performance Polymers
Trade Name Hytrel®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Hytrel® HTR8785 BK482 Polyester Elastomer TPC-ET  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 34.0 MPa
4930 psi
ISO 527-1/-2
Tensile Stress 16.6 MPa

@Strain 10.0 %
2410 psi

@Strain 10.0 %
ISO 527-1/-2
Elongation at Break 300 %
300 %
ISO 527-1/-2
Tensile Modulus 0.262 GPa
38.0 ksi
ISO 527-1/-2
Thermal Properties Metric English Comments
Melting Point 209 °C
408 °F
10°C/min; ISO 11357-1/-3
Descriptive Properties Value Comments
Delivery Form Pellets
Part Marking Code >TPC-ET<
ISO 11469
Processing Injection Moulding
Other Extrusion
Profile Extrusion
Sheet Extrusion
Regional Availability Asia Pacific
Europe
Global
Near East/Africa
North America
South and Central America
Resin Identification TPC-ET
ISO 1043
Special Characteristics Heat stabilised or stable to heat
U.V. stabilised or stable to weather
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved