Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Performance Polymers Rynite® 530 BK503 Polyethylene Terephthalate (PET)  (Unverified Data**)

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), 30% Glass Reinforced
Manufacturer DuPont Performance Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Rynite® 530 BK503 Polyethylene Terephthalate (PET)  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
30% Glass Reinforced Polyethylene Terephthalate Rynite 530 BK503 is a 30% glass reinforced modified polyethylene terephthalate with outstanding balance of strength stiffness and toughness excellent electrical properties surface appearance and chemicalInformation provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.56 g/cc
0.0564 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0030 cm/cm
0.0030 in/in
ISO 294-4 2577
Linear Mold Shrinkage, Transverse 0.0090 cm/cm
0.0090 in/in
ISO 294-4 2577
Mechanical Properties Metric English Comments
Tensile Strength at Break 150 MPa
21800 psi
ISO 527-1/-2
Elongation at Break 2.1 %
2.1 %
ISO 527-1/-2
Tensile Modulus 10.2 GPa
1480 ksi
ISO 527-1/-2
Flexural Strength 210 MPa
30500 psi
ISO 178
Flexural Modulus 8.94 GPa
1300 ksi
ISO 178
Izod Impact, Notched (ISO) 9.50 kJ/m²
4.52 ft-lb/in²
ISO 180/1A
8.50 kJ/m²

@Temperature -40.0 °C
4.04 ft-lb/in²

@Temperature -40.0 °F
ISO 180/1A
Izod Impact, Unnotched (ISO) 45.0 kJ/m²
21.4 ft-lb/in²
ISO 180/1U
35.0 kJ/m²

@Temperature -40.0 °C
16.7 ft-lb/in²

@Temperature -40.0 °F
ISO 180/1U
Charpy Impact Unnotched 5.20 J/cm²
24.7 ft-lb/in²
ISO 179/1eU
4.50 J/cm²

@Temperature -40.0 °C
21.4 ft-lb/in²

@Temperature -40.0 °F
ISO 179/1eU
Charpy Impact, Notched 0.950 J/cm²
4.52 ft-lb/in²
ISO 179/1eA
0.800 J/cm²

@Temperature -40.0 °C
3.81 ft-lb/in²

@Temperature -40.0 °F
ISO 179/1eA
0.850 J/cm²

@Temperature -30.0 °C
4.04 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 244 °C
471 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 221 °C
430 °F
ISO 75-1/-2
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
IEC 60695-11-10
HB

@Thickness 0.800 mm
HB

@Thickness 0.0315 in
IEC 60695-11-10
Flame Spread 38 mm/min

@Thickness 1.00 mm
1.5 in/min

@Thickness 0.0394 in
ISO 3795 (FMVSS 302)
Electrical Properties Metric English Comments
Dielectric Strength 32.0 kV/mm
813 kV/in
IEC 60243-1
Descriptive Properties Value Comments
Part Marking Code >PET-GF30<
ISO 11469
Processing Injection Moulding
Regional Availability Asia Pacific
Europe
Global
Near East/Africa
North America
South and Central America
Resin Identification PET-GF30
UL recognition UL