DuPont Performance Polymers Rynite® 545 BK504 Polyethylene Terephthalate (PET)  (Unverified Data**)

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), 50% Glass Reinforced
Manufacturer DuPont Performance Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Rynite® 545 BK504 Polyethylene Terephthalate (PET)  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
45% Glass Reinforced Polyethylene Terephthalate Rynite 545 BK504 is a 45% glass reinforced modified polyethylene terephthalate with good strength and stiffness excellent dimensional stability and creep resistance.Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.70 g/cc
0.0614 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0020 cm/cm
0.0020 in/in
ISO 294-4 2577
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
0.0080 in/in
ISO 294-4 2577
Mechanical Properties Metric English Comments
Tensile Strength at Break 175 MPa
25400 psi
ISO 527-1/-2
Elongation at Break 1.9 %
1.9 %
ISO 527-1/-2
Tensile Modulus 15.5 GPa
2250 ksi
ISO 527-1/-2
Flexural Modulus 14.0 GPa
2030 ksi
ISO 178
Charpy Impact Unnotched 6.00 J/cm²
28.6 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 1.10 J/cm²
5.23 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 17.0 µm/m-°C
9.44 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 85.0 µm/m-°C
47.2 µin/in-°F
ISO 11359-1/-2
Melting Point 249 °C
480 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 230 °C
446 °F
ISO 75-1/-2
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
IEC 60695-11-10
HB

@Thickness 0.800 mm
HB

@Thickness 0.0315 in
IEC 60695-11-10
Descriptive Properties Value Comments
Part Marking Code >PET-GF45<
ISO 11469
Processing Injection Moulding
Regional Availability Asia Pacific
Europe
Global
Near East/Africa
North America
South and Central America
Resin Identification PET-GF45
UL recognition UL