Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), 40% Glass Reinforced
Manufacturer DuPont Performance Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Rynite® RE15022 NC010 Polyethylene Terephthalate (PET).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
36% Glass Reinforced Polyethylene TerephthalateRynite RE15022 NC010 is a 36% glass reinforced product designed for applications that need high burst strength.Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Specific Gravity 1.65 g/cc
1.65 g/cc
ASTM D792
Density 1.65 g/cc
0.0596 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 205 MPa
29700 psi
ISO 527-1/-2
Tensile Strength 195 MPa
28300 psi
ASTM D638
Elongation at Break 2.4 %
2.4 %
ISO 527-1/-2
2.4 %
2.4 %
ASTM D638
Tensile Modulus 14.0 GPa
2030 ksi
ISO 527-1/-2
Izod Impact, Unnotched (ISO) 1180 kJ/m²
561 ft-lb/in²
ASTM D4812
Izod Impact Resistance 10.5 J/cm²
50.0 ft-lb/in²
ASTM D256
11.0 J/cm²
52.4 ft-lb/in²
ASTM D256
Charpy Impact Unnotched 6.50 J/cm²
30.9 ft-lb/in²
ISO 179/1eU
Thermal Properties Metric English Comments
Melting Point 247 °C
477 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 235 °C
455 °F
ISO 75-1/-2
235 °C
455 °F
ASTM D648
Descriptive Properties Value Comments
Delivery Form Pellets
Processing Injection Moulding
Regional Availability Asia Pacific
Europe
Global
Near East/Africa
North America