Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Performance Polymers Rynite® RE19051 BK507 Polyethylene Terephthalate (PET)

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), Glass/Mineral Reinforced
Manufacturer DuPont Performance Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Rynite® RE19051 BK507 Polyethylene Terephthalate (PET).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
40% Glass/Mineral Reinforced Flame Retardant Polyethylene Terephthalate Rynite RE19051 BK507 is a 40% glass and mineral reinforced flame retardant polyethylene terephthalate black resin.Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.73 g/cc
0.0625 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0020 cm/cm
0.0020 in/in
ISO 294-4 2577
Linear Mold Shrinkage, Transverse 0.0090 cm/cm
0.0090 in/in
ISO 294-4 2577
Melt Flow 70 g/10 min

@Load 5.00 kg,
Temperature 280 °C
70 g/10 min

@Load 11.0 lb,
Temperature 536 °F
cm³/10min; ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 110 MPa
16000 psi
ISO 527-1/-2
Tensile Strength 195 MPa
28300 psi
ASTM D638
Elongation at Break 1.7 %
1.7 %
ISO 527-1/-2
2.4 %
2.4 %
ASTM D638
Tensile Modulus 11.0 GPa
1600 ksi
ISO 527-1/-2
Flexural Strength 170 MPa
24700 psi
ISO 178
Flexural Modulus 9.70 GPa
1410 ksi
ISO 178
Charpy Impact, Notched 0.650 J/cm²
3.09 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 23.0 µm/m-°C
12.8 µin/in-°F
ISO 11359-1/-2
0.140 µm/m-°C

@Temperature 55.0 - 160 °C
0.0778 µin/in-°F

@Temperature 131 - 320 °F
ISO 11359-1/-2
23.0 µm/m-°C

@Temperature -40.0 - 23.0 °C
12.8 µin/in-°F

@Temperature -40.0 - 73.4 °F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 78.0 µm/m-°C
43.3 µin/in-°F
ISO 11359-1/-2
0.610 µm/m-°C

@Temperature -40.0 - 23.0 °C
0.339 µin/in-°F

@Temperature -40.0 - 73.4 °F
ISO 11359-1/-2
1.10 µm/m-°C

@Temperature 55.0 - 160 °C
0.611 µin/in-°F

@Temperature 131 - 320 °F
ISO 11359-1/-2
Melting Point 247 °C
477 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 214 °C
417 °F
ISO 75-1/-2
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
IEC 60695-11-10
V-0

@Thickness 0.800 mm
V-0

@Thickness 0.0315 in
IEC 60695-11-10
5VA

@Thickness 0.800 mm
5VA

@Thickness 0.0315 in
IEC 60695-11-20
Electrical Properties Metric English Comments
Volume Resistivity 5.00e+14 ohm-cm
5.00e+14 ohm-cm
IEC 60093
Surface Resistance >= 1.00e+15 ohm
>= 1.00e+15 ohm
IEC 60093
Descriptive Properties Value Comments
Delivery Form Pellets
Part Marking Code >PET-(MD+GF)40FR<
ISO 11469
Processing Injection Moulding
Regional Availability Asia Pacific
Resin Identification PET-(MD+GF)40FR(17)
UL recognition UL
Copyright © lookpolymers.com All Rights Reserved