DuPont Performance Polymers VESPEL TP-8130 Polyimide

Category Polymer , Thermoplastic , Polyimide, Thermoplastic
Manufacturer DuPont Performance Polymers
Trade Name VESPEL
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers VESPEL TP-8130 Polyimide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DuPont Vespel TP-8130 parts are specified for mechanical, thermal, and tribological properties. TP-8130 parts exhibits excellent strength and toughness, dimensional stability, low outgassing, radiation resistance, creep resistance, and low coefficient ofInformation provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Specific Gravity 1.42 g/cc
1.42 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength 144 MPa

@Temperature 150 °C
20900 psi

@Temperature 302 °F
ASTM D638
Elongation at Break 2.0 %

@Temperature 23.0 °C
2.0 %

@Temperature 73.4 °F
ASTM D638
4.0 %

@Temperature 150 °C
4.0 %

@Temperature 302 °F
ASTM D638
Flexural Strength 314 MPa

@Temperature 23.0 °C
45500 psi

@Temperature 73.4 °F
ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 248 °C
478 °F
ASTM D648
Descriptive Properties Value Comments
Appearance Natural Color
Forms Shapes
Material Status Current
Region Available - Global Yes
RoHS Compliance Contact Manufacturer