DuPont Performance Polymers VESPEL TP-8161 Polyimide

Category Polymer , Thermoplastic , Polyimide, Thermoplastic
Manufacturer DuPont Performance Polymers
Trade Name VESPEL
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers VESPEL TP-8161 Polyimide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DuPont Vespel TP-8161 parts are specified for high-temperature applications. TP-8161 parts offer a unique balance of mechanical and thermal properties for superior performance in aggressive environments. TP-8161 parts are produced from unfilled thermoplasInformation provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Specific Gravity 1.35 g/cc

@Temperature 23.0 °C
1.35 g/cc

@Temperature 73.4 °F
ASTM D792
Water Absorption 0.070 %

@Temperature 23.0 °C
0.070 %

@Temperature 73.4 °F
60%RH,23°C,24h; ASTM D570
0.16 %

@Temperature 23.0 °C
0.16 %

@Temperature 73.4 °F
50%RH,23°C,24h; ASTM D570
Mechanical Properties Metric English Comments
Tensile Strength 80.0 MPa

@Temperature 23.0 °C
11600 psi

@Temperature 73.4 °F
ASTM D638
Elongation at Break 3.0 %

@Temperature 23.0 °C
3.0 %

@Temperature 73.4 °F
ASTM D638
Flexural Strength 154 MPa

@Temperature 23.0 °C
22300 psi

@Temperature 73.4 °F
ASTM D790
Flexural Modulus 0.00420 GPa

@Temperature 23.0 °C
0.609 ksi

@Temperature 73.4 °F
ASTM D790
Izod Impact, Notched 0.370 J/cm

@Temperature 23.0 °C
0.693 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 295 °C
563 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 0.400 mm
V-0

@Thickness 0.0157 in
DAM; UL94
5VA

@Thickness 2.00 mm
5VA

@Thickness 0.0787 in
DAM; UL94
Oxygen Index 47 %
47 %
ASTM D2863
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+17 - 1.00e+18 ohm-cm

@Temperature 23.0 °C
1.00e+17 - 1.00e+18 ohm-cm

@Temperature 73.4 °F
ASTM D257
Surface Resistance 1.00e+15 - 1.00e+16 ohm

@Temperature 23.0 °C
1.00e+15 - 1.00e+16 ohm

@Temperature 73.4 °F
ASTM D257
Dielectric Constant 3.1

@Frequency 1.00e+6 Hz,
Temperature 23.0 °C
3.1

@Frequency 1.00e+6 Hz,
Temperature 73.4 °F
ASTM D150
3.2

@Frequency 10000 Hz,
Temperature 23.0 °C
3.2

@Frequency 10000 Hz,
Temperature 73.4 °F
ASTM D150
Dissipation Factor 0.00090

@Frequency 10000 Hz,
Temperature 23.0 °C
0.00090

@Frequency 10000 Hz,
Temperature 73.4 °F
ASTM D150
0.0030

@Frequency 1.00e+6 Hz,
Temperature 23.0 °C
0.0030

@Frequency 1.00e+6 Hz,
Temperature 73.4 °F
ASTM D150
Descriptive Properties Value Comments
Appearance Natural Color
Forms Shapes
Material Status Current
Region Available - Global Yes
RoHS Compliance Contact Manufacturer