Material Notes:
Thermoplastic parts from filled PI (polyimide) for balanced mechanical properties and low wear and friction performance in high temperature hostile environmentsInformation provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Specific Gravity 1.46 g/cc

@Temperature 23.0 °C
1.46 g/cc

@Temperature 73.4 °F
ASTM D792
Water Absorption 0.20 %

@Temperature 23.0 °C
0.20 %

@Temperature 73.4 °F
50%RH,23°C,24h; ASTM D570
0.20 %

@Temperature 23.0 °C
0.20 %

@Temperature 73.4 °F
Immersion 24h; ASTM D570
Mechanical Properties Metric English Comments
Tensile Strength 106 MPa

@Temperature 150 °C
15400 psi

@Temperature 302 °F
ASTM D638
142 MPa

@Temperature 23.0 °C
20600 psi

@Temperature 73.4 °F
ASTM D638
Elongation at Break 1.7 %

@Temperature 150 °C
1.7 %

@Temperature 302 °F
ASTM D638
Flexural Strength 130 MPa

@Temperature 150 °C
18900 psi

@Temperature 302 °F
ASTM D790
Flexural Modulus 0.0102 GPa

@Temperature 150 °C
1.48 ksi

@Temperature 302 °F
ASTM D790
Izod Impact, Notched 0.640 J/cm

@Temperature 23.0 °C
1.20 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Izod Impact, Unnotched 3.308 J/cm

@Temperature 23.0 °C
6.197 ft-lb/in

@Temperature 73.4 °F
ASTM D4812
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 8.00 µm/m-°C

@Temperature 150 °C
4.44 µin/in-°F

@Temperature 302 °F
ASTM E 228
CTE, linear, Transverse to Flow 36.0 µm/m-°C

@Temperature 150 °C
20.0 µin/in-°F

@Temperature 302 °F
ASTM E 228
Deflection Temperature at 1.8 MPa (264 psi) 244 °C
471 °F
ASTM D648
Glass Transition Temp, Tg 249 °C
480 °F
ASTM D3418
Descriptive Properties Value Comments
Appearance Natural Color
Forms Shapes
Heat Stabilized Yes
Material Status Current
Polymer Family Polyimide
Polymer Type PI
Region Available - Global Yes
RoHS Compliance Contact Manufacturer
Ultrasonic Weldable Yes