Material Notes:
DuPont Vespel TP-8792 parts are specified for mechanical, thermal, and tribological properties. TP-8792 offers excellent strength and toughness, dimensional stability, low outgassing, radiation resistance, creep resistance, and low coefficient of thermalInformation provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Specific Gravity 1.44 g/cc
1.44 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength 170 MPa

@Temperature 23.0 °C
24700 psi

@Temperature 73.4 °F
ASTM D638
Elongation at Break 5.0 %

@Temperature 23.0 °C
5.0 %

@Temperature 73.4 °F
ASTM D638
Flexural Strength 230 MPa

@Temperature 23.0 °C
33400 psi

@Temperature 73.4 °F
ASTM D790
Flexural Modulus 10.8 GPa

@Temperature 23.0 °C
1570 ksi

@Temperature 73.4 °F
ASTM D790
Izod Impact, Notched 1.10 J/cm

@Temperature 23.0 °C
2.06 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 52.0 µm/m-°C

@Temperature 23.0 - 150 °C
28.9 µin/in-°F

@Temperature 73.4 - 302 °F
ASTM E 228
Deflection Temperature at 1.8 MPa (264 psi) 246 °C
475 °F
ASTM D648
Descriptive Properties Value Comments
Appearance Natural Color