DuPont Performance Polymers VTR 8600 (GF-S) Peroxide Cured Fluoroelastomer (FKM)  (discontinued **)

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers VTR 8600 (GF-S) Peroxide Cured Fluoroelastomer (FKM)  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FormulationVTR-8600
Mechanical Properties Metric English Comments
Hardness, Shore A 72
72
Cured 7 min at 177°C and Post Cured 2 hr at 232°C
Tensile Strength, Ultimate 20.7 MPa
3000 psi
Cured 7 min at 177°C and Post Cured 2 hr at 232°C
Elongation at Break 269 %
269 %
Cured 7 min at 177°C and Post Cured 2 hr at 232°C
Modulus of Elasticity 0.000700 GPa
0.102 ksi
10% Modulus, Cured 7 min at 177°C and Post Cured 2 hr at 232°C
100% Modulus 0.00540 GPa
0.783 ksi
Cured 7 min at 177°C and Post Cured 2 hr at 232°C
Compression Set 17 %

@Temperature 200 °C
17 %

@Temperature 392 °F
Method B, O-rings 22 hr at 200°C (Post Cured 2 hr at 232°C)