Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Performance Polymers Zytel® 70G13HS1L BK031 Nylon 66  (Unverified Data**)

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 10% Glass Fiber Filled
Manufacturer DuPont Performance Polymers
Trade Name Zytel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Zytel® 70G13HS1L BK031 Nylon 66  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
13% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G13HS1L BK031 is a 13% glass fiber reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0444 lb/in³
DAM; ISO 1183
Linear Mold Shrinkage, Flow 0.0050 cm/cm
0.0050 in/in
DAM; ISO 294-4 2577
Linear Mold Shrinkage, Transverse 0.010 cm/cm
0.010 in/in
DAM; ISO 294-4 2577
Mechanical Properties Metric English Comments
Tensile Strength at Break 75.0 MPa
10900 psi
50%RH; ISO 527-1/-2
120 MPa
17400 psi
DAM; ISO 527-1/-2
Elongation at Break 2.7 %
2.7 %
DAM; ISO 527-1/-2
12 %
12 %
50%RH; ISO 527-1/-2
Tensile Modulus 3.50 GPa
508 ksi
50%RH; ISO 527-1/-2
5.50 GPa
798 ksi
DAM; ISO 527-1/-2
Flexural Strength 100 MPa
14500 psi
50%RH; ISO 178
190 MPa
27600 psi
DAM; ISO 178
Flexural Modulus 4.90 GPa
711 ksi
DAM; ISO 178
Izod Impact, Notched (ISO) 4.50 kJ/m²
2.14 ft-lb/in²
DAM; ISO 180/1A
4.50 kJ/m²

@Temperature -40.0 °C
2.14 ft-lb/in²

@Temperature -40.0 °F
DAM; ISO 180/1A
Charpy Impact, Notched 0.500 J/cm²
2.38 ft-lb/in²
DAM; ISO 179/1eA
0.450 J/cm²

@Temperature -40.0 °C
2.14 ft-lb/in²

@Temperature -40.0 °F
DAM; ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 40.0 µm/m-°C
22.2 µin/in-°F
DAM; ISO 11359-1/-2
CTE, linear, Transverse to Flow 96.0 µm/m-°C
53.3 µin/in-°F
DAM; ISO 11359-1/-2
Melting Point 262 °C
504 °F
DAM; 10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 258 °C
496 °F
DAM; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 238 °C
460 °F
DAM; ISO 75-1/-2
Flammability, UL94 HB

@Thickness 0.700 mm
HB

@Thickness 0.0276 in
DAM; IEC 60695-11-10
Descriptive Properties Value Comments
Part Marking Code >PA66-GF13<
ISO 11469
Processing Injection Moulding
Regional Availability Asia Pacific
Europe
Global
Near East/Africa
North America
South and Central America
Resin Identification PA66-GF13
Special Characteristics Heat stabilised or stable to heat