DuPont Performance Polymers Zytel® 70G30HSLR BK099 Nylon 66  (Unverified Data**)

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer DuPont Performance Polymers
Trade Name Zytel®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Zytel® 70G30HSLR BK099 Nylon 66  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
30% Glass Reinforced Heat Stabilized Hydrolysis Resistant Polyamide 66 Zytel 70G30HSLR BK099 is a 30% glass fiber reinforced heat stabilized hydrolysis resistant polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.37 g/cc
0.0495 lb/in³
DAM; ISO 1183
Viscosity 43340 cP

@Shear Rate 5000 1/s,
Temperature 305 °C
43340 cP

@Shear Rate 5000 1/s,
Temperature 581 °F
ISO 11403-1 -2
54070 cP

@Shear Rate 5000 1/s,
Temperature 295 °C
54070 cP

@Shear Rate 5000 1/s,
Temperature 563 °F
ISO 11403-1 -2
68870 cP

@Shear Rate 5000 1/s,
Temperature 285 °C
68870 cP

@Shear Rate 5000 1/s,
Temperature 545 °F
ISO 11403-1 -2
127100 cP

@Shear Rate 500 1/s,
Temperature 305 °C
127100 cP

@Shear Rate 500 1/s,
Temperature 581 °F
ISO 11403-1 -2
162500 cP

@Shear Rate 500 1/s,
Temperature 295 °C
162500 cP

@Shear Rate 500 1/s,
Temperature 563 °F
ISO 11403-1 -2
210550 cP

@Shear Rate 500 1/s,
Temperature 285 °C
210550 cP

@Shear Rate 500 1/s,
Temperature 545 °F
ISO 11403-1 -2
Linear Mold Shrinkage, Flow 0.0030 cm/cm
0.0030 in/in
DAM; ISO 294-4 2577
Linear Mold Shrinkage, Transverse 0.010 cm/cm
0.010 in/in
DAM; ISO 294-4 2577
Mechanical Properties Metric English Comments
Tensile Strength at Break 130 MPa
18900 psi
50%RH; ISO 527-1/-2
195 MPa
28300 psi
DAM; ISO 527-1/-2
Elongation at Break 3.0 %
3.0 %
DAM; ISO 527-1/-2
5.0 %
5.0 %
50%RH; ISO 527-1/-2
Tensile Modulus 7.20 GPa
1040 ksi
50%RH; ISO 527-1/-2
10.0 GPa
1450 ksi
DAM; ISO 527-1/-2
3.322 GPa

@Temperature 180 °C
481.8 ksi

@Temperature 356 °F
DAM; Dynamic; ISO 11403-1 -2
4.515 GPa

@Temperature 100 °C
654.8 ksi

@Temperature 212 °F
DAM; Dynamic; ISO 11403-1 -2
8.659 GPa

@Temperature 50.0 °C
1256 ksi

@Temperature 122 °F
DAM; Dynamic; ISO 11403-1 -2
9.283 GPa

@Temperature 10.0 °C
1346 ksi

@Temperature 50.0 °F
DAM; Dynamic; ISO 11403-1 -2
9.365 GPa

@Temperature -20.0 °C
1358 ksi

@Temperature -4.00 °F
DAM; Dynamic; ISO 11403-1 -2
Shear Modulus 1.292 GPa

@Temperature 170 °C
187.4 ksi

@Temperature 338 °F
DAM; Dynamic; ISO 11403-1 -2
1.473 GPa

@Temperature 130 °C
213.6 ksi

@Temperature 266 °F
DAM; Dynamic; ISO 11403-1 -2
2.105 GPa

@Temperature 80.0 °C
305.3 ksi

@Temperature 176 °F
DAM; Dynamic; ISO 11403-1 -2
3.441 GPa

@Temperature 30.0 °C
499.1 ksi

@Temperature 86.0 °F
DAM; Dynamic; ISO 11403-1 -2
3.465 GPa

@Temperature 10.0 °C
502.6 ksi

@Temperature 50.0 °F
DAM; Dynamic; ISO 11403-1 -2
3.494 GPa

@Temperature -20.0 °C
506.8 ksi

@Temperature -4.00 °F
DAM; Dynamic; ISO 11403-1 -2
Izod Impact, Notched (ISO) 12.0 kJ/m²
5.71 ft-lb/in²
DAM; ISO 180/1A
14.0 kJ/m²
6.66 ft-lb/in²
50%RH; ISO 180/1A
Charpy Impact Unnotched 7.50 J/cm²
35.7 ft-lb/in²
DAM; ISO 179/1eU
9.00 J/cm²
42.8 ft-lb/in²
50%RH; ISO 179/1eU
Charpy Impact, Notched 1.20 J/cm²
5.71 ft-lb/in²
DAM; ISO 179/1eA
1.40 J/cm²
6.66 ft-lb/in²
50%RH; ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 262 °C
504 °F
DAM; 10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 253 °C
487 °F
DAM; ISO 75-1/-2
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
DAM; IEC 60695-11-10
HB

@Thickness 0.800 mm
HB

@Thickness 0.0315 in
DAM; IEC 60695-11-10
Flame Spread 24 mm/min

@Thickness 1.00 mm
0.94 in/min

@Thickness 0.0394 in
SE/B24; ISO 3795 (FMVSS 302)
Electrical Properties Metric English Comments
Comparative Tracking Index 400 V
400 V
DAM; IEC 60112
400 - 600 V
400 - 600 V
DAM; UL 746A
Descriptive Properties Value Comments
Odour class 4
VDA 270
Part Marking Code >PA66-GF30<
ISO 11469
Processing Injection Moulding
Regional Availability Asia Pacific
Europe
Global
Near East/Africa
North America
South and Central America
Resin Identification PA66-GF30
Special Characteristics Heat stabilised or stable to heat
UL recognition UL
DAM