DuPont Performance Polymers Zytel® 70G43HSLA BK099 Nylon 66  (Unverified Data**)

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 40% Glass Fiber Filled
Manufacturer DuPont Performance Polymers
Trade Name Zytel®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Zytel® 70G43HSLA BK099 Nylon 66  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
43% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G43HSLA BK099 is a 43% glass fiber reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.49 g/cc
0.0538 lb/in³
DAM; ISO 1183
Water Absorption 7.6 %

@Thickness 2.00 mm
7.6 %

@Thickness 0.0787 in
DAM; Sim. to ISO 62
Moisture Absorption 2.20 %

@Thickness 2.00 mm
2.20 %

@Thickness 0.0787 in
DAM; Sim. to ISO 62
Viscosity Test 120 cm³/g
120 cm³/g
DAM; ISO 307 1157 1628
Linear Mold Shrinkage, Flow 0.0030 cm/cm
0.0030 in/in
DAM; ISO 294-4 2577
Linear Mold Shrinkage, Transverse 0.0090 cm/cm
0.0090 in/in
DAM; ISO 294-4 2577
Mechanical Properties Metric English Comments
Tensile Strength at Break 160 MPa
23200 psi
50%RH; ISO 527-1/-2
225 MPa
32600 psi
DAM; ISO 527-1/-2
Elongation at Break 2.5 %
2.5 %
DAM; ISO 527-1/-2
3.5 %
3.5 %
50%RH; ISO 527-1/-2
Tensile Modulus 11.0 GPa
1600 ksi
50%RH; ISO 527-1/-2
14.0 GPa
2030 ksi
DAM; ISO 527-1/-2
Izod Impact, Notched (ISO) 14.0 kJ/m²
6.66 ft-lb/in²
DAM; ISO 180/1A
16.0 kJ/m²
7.61 ft-lb/in²
50%RH; ISO 180/1A
Charpy Impact Unnotched 9.00 J/cm²
42.8 ft-lb/in²
DAM; ISO 179/1eU
9.50 J/cm²
45.2 ft-lb/in²
50%RH; ISO 179/1eU
Charpy Impact, Notched 1.60 J/cm²
7.61 ft-lb/in²
DAM; ISO 179/1eA
1.80 J/cm²
8.57 ft-lb/in²
50%RH; ISO 179/1eA
Puncture Energy 4.40 J
3.25 ft-lb
DAM; ISO 6603-2
Thermal Properties Metric English Comments
Thermal Conductivity 0.250 W/m-K
1.74 BTU-in/hr-ft²-°F
of melt
Melting Point 262 °C
504 °F
DAM; 10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 258 °C
496 °F
DAM; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 255 °C
491 °F
DAM; ISO 75-1/-2
Glass Transition Temp, Tg 80.0 °C
176 °F
DAM; 10°C/min; ISO 11357-1/-2
Oxygen Index 24 %
24 %
DAM; ISO 4589-1/-2
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
DAM; IEC 60093
Dielectric Strength 25.0 kV/mm
635 kV/in
DAM; IEC 60243-1
Dissipation Factor 0.013

@Frequency 100 Hz
0.013

@Frequency 100 Hz
DAM; IEC 60250
0.015

@Frequency 1.00e+6 Hz
0.015

@Frequency 1.00e+6 Hz
DAM; IEC 60250
Comparative Tracking Index 600 V
600 V
DAM; IEC 60112
Descriptive Properties Value Comments
Additives Release agent
Delivery Form Pellets
Part Marking Code >PA66-GF43<
ISO 11469
Processing Injection Moulding
Regional Availability Asia Pacific
Europe
Global
Near East/Africa
North America
South and Central America
Resin Identification PA66-GF43
Special Characteristics Heat stabilised or stable to heat