DuPont Performance Polymers Zytel® 73G30TGI BK267 Nylon 6  (Unverified Data**)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 30% Glass Fiber Filled
Manufacturer DuPont Performance Polymers
Trade Name Zytel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Zytel® 73G30TGI BK267 Nylon 6  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Zytel® 73G30TGI BK267 is a 30% glass fiber reinforced, toughened, black polyamide 6 optimized for gas injection molding process.Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.35 g/cc

@Temperature 23.0 °C
0.0488 lb/in³

@Temperature 73.4 °F
DAM; ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 163 MPa

@Temperature 23.0 °C
23600 psi

@Temperature 73.4 °F
DAM; ISO 527
Elongation at Break 3.3 %

@Temperature 23.0 °C
3.3 %

@Temperature 73.4 °F
DAM; ISO 527
Tensile Modulus 9.40 GPa

@Temperature 23.0 °C
1360 ksi

@Temperature 73.4 °F
DAM; ISO 527
Flexural Strength 260 MPa

@Temperature 23.0 °C
37700 psi

@Temperature 73.4 °F
DAM; ISO 178
Flexural Modulus 8.80 GPa

@Temperature 23.0 °C
1280 ksi

@Temperature 73.4 °F
DAM; ISO 178
Izod Impact, Notched (ISO) 11.0 kJ/m²

@Temperature -40.0 °C
5.23 ft-lb/in²

@Temperature -40.0 °F
DAM; ISO 180/1A
16.0 kJ/m²

@Temperature 23.0 °C
7.61 ft-lb/in²

@Temperature 73.4 °F
DAM; ISO 180/1A
Charpy Impact, Notched 1.40 J/cm²

@Temperature 23.0 °C
6.66 ft-lb/in²

@Temperature 73.4 °F
DAM; ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 220 °C

@Temperature 23.0 °C
428 °F

@Temperature 73.4 °F
DAM; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 206 °C
403 °F
DAM; ISO 75-1/-2
Processing Properties Metric English Comments
Melt Temperature 270 °C
518 °F
DAM; Optimum
260 - 280 °C
500 - 536 °F
DAM
Mold Temperature 70.0 - 120 °C
158 - 248 °F
DAM
100 °C
212 °F
DAM; optimum
Drying Temperature 80.0 °C
176 °F
DAM
Dry Time 2.00 - 4.00 hour
2.00 - 4.00 hour
DAM
Moisture Content <= 0.20 %
<= 0.20 %
DAM
Descriptive Properties Value Comments
Appearance Black Color
DAM
Forms Pellets
DAM
Generic PA6
DAM
Material Status Preliminary Data
DAM
Processing Method Injection Molding
DAM
Product Category Gas Injection Resins
DAM
Glass Reinforced Resins
DAM
Toughened Resins
DAM