Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Performance Polymers Zytel® 80G25HS BK117 Nylon 66  (Unverified Data**)

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer DuPont Performance Polymers
Trade Name Zytel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Zytel® 80G25HS BK117 Nylon 66  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
25% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G25HS BK117 is a 25% glass fiber reinforced toughened heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.25 g/cc
0.0452 lb/in³
DAM; ISO 1183
Viscosity Test 140 cm³/g
140 cm³/g
DAM; ISO 307 1157 1628
Linear Mold Shrinkage, Flow 0.0030 cm/cm
0.0030 in/in
DAM; ISO 294-4 2577
Mechanical Properties Metric English Comments
Tensile Strength at Break 87.0 MPa
12600 psi
50%RH; ISO 527-1/-2
122 MPa
17700 psi
DAM; ISO 527-1/-2
Elongation at Break 4.0 %
4.0 %
DAM; ISO 527-1/-2
8.0 %
8.0 %
50%RH; ISO 527-1/-2
Tensile Modulus 4.70 GPa
682 ksi
50%RH; ISO 527-1/-2
6.90 GPa
1000 ksi
DAM; ISO 527-1/-2
Flexural Modulus 6.00 GPa
870 ksi
DAM; ISO 178
Izod Impact, Notched (ISO) 20.0 kJ/m²
9.52 ft-lb/in²
DAM; ISO 180/1A
23.0 kJ/m²
10.9 ft-lb/in²
50%RH; ISO 180/1A
12.0 kJ/m²

@Temperature -30.0 °C
5.71 ft-lb/in²

@Temperature -22.0 °F
50%RH; ISO 180/1A
12.0 kJ/m²

@Temperature -40.0 °C
5.71 ft-lb/in²

@Temperature -40.0 °F
50%RH; ISO 180/1A
13.0 kJ/m²

@Temperature -40.0 °C
6.19 ft-lb/in²

@Temperature -40.0 °F
DAM; ISO 180/1A
13.0 kJ/m²

@Temperature -30.0 °C
6.19 ft-lb/in²

@Temperature -22.0 °F
DAM; ISO 180/1A
Charpy Impact Unnotched 8.10 J/cm²
38.5 ft-lb/in²
50%RH; ISO 179/1eU
8.30 J/cm²
39.5 ft-lb/in²
DAM; ISO 179/1eU
8.70 J/cm²

@Temperature -30.0 °C
41.4 ft-lb/in²

@Temperature -22.0 °F
50%RH; ISO 179/1eU
8.90 J/cm²

@Temperature -30.0 °C
42.4 ft-lb/in²

@Temperature -22.0 °F
DAM; ISO 179/1eU
Charpy Impact, Notched 2.20 J/cm²
10.5 ft-lb/in²
DAM; ISO 179/1eA
2.40 J/cm²
11.4 ft-lb/in²
50%RH; ISO 179/1eA
1.30 J/cm²

@Temperature -30.0 °C
6.19 ft-lb/in²

@Temperature -22.0 °F
50%RH; ISO 179/1eA
1.40 J/cm²

@Temperature -30.0 °C
6.66 ft-lb/in²

@Temperature -22.0 °F
DAM; ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 262 °C
504 °F
DAM; 10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 258 °C
496 °F
DAM; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 240 °C
464 °F
DAM; ISO 75-1/-2
Descriptive Properties Value Comments
Part Marking Code >PA66-IGF25<
ISO 11469
Processing Injection Moulding
Regional Availability Asia Pacific
Europe
Global
Near East/Africa
North America
South and Central America
Resin Identification PA66-IGF25
Special Characteristics Heat stabilised or stable to heat
Copyright © lookpolymers.com All Rights Reserved