Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Performance Polymers Zytel® BM7300THS BK317 Nylon 6  (Unverified Data**)

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer DuPont Performance Polymers
Trade Name Zytel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Zytel® BM7300THS BK317 Nylon 6  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Zytel® BM7300THS is an unreinforced, heat stabilized, lubricated, toughened polyamide 6 for blow molding.Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Specific Gravity 1.09 g/cc
1.09 g/cc
DAM; ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Yield 60.0 MPa

@Temperature 23.0 °C
8700 psi

@Temperature 73.4 °F
DAM; ISO 527
Elongation at Break 160 %

@Temperature 23.0 °C
160 %

@Temperature 73.4 °F
DAM; ISO 527
>= 160 %

@Temperature 23.0 °C
>= 160 %

@Temperature 73.4 °F
50%RH; ISO 527
Elongation at Yield 4.4 %

@Temperature 23.0 °C
4.4 %

@Temperature 73.4 °F
DAM; ISO 527
Tensile Modulus 0.570 GPa

@Temperature 23.0 °C
82.7 ksi

@Temperature 73.4 °F
50%RH; ISO 527
2.17 GPa

@Temperature 23.0 °C
315 ksi

@Temperature 73.4 °F
DAM; ISO 527
Charpy Impact, Notched 2.20 J/cm²

@Temperature -30.0 °C
10.5 ft-lb/in²

@Temperature -22.0 °F
50%RH; ISO 179/1eA
2.30 J/cm²

@Temperature -30.0 °C
10.9 ft-lb/in²

@Temperature -22.0 °F
DAM; ISO 179/1eA
8.20 J/cm²

@Temperature 23.0 °C
39.0 ft-lb/in²

@Temperature 73.4 °F
DAM; ISO 179/1eA
15.0 J/cm²

@Temperature 23.0 °C
71.4 ft-lb/in²

@Temperature 73.4 °F
50%RH; ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 221 °C
430 °F
10°C/min; DAM; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 117 °C
243 °F
DAM; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 52.0 °C
126 °F
DAM; ISO 75-1/-2
Descriptive Properties Value Comments
Appearance Black Color
DAM
Forms Pellets
DAM
Generic Nylon 6
DAM
Material Status Preliminary Data
DAM
Processing Method Blow Molding
DAM
Product Category Blow Moldable Resins
DAM
Unreinforced Resins
DAM
Region Available - Global Yes
DAM
RoHS Compliance Contact Manufacturer
DAM