DuPont Performance Polymers Zytel® HTN 52G45HSL BK083 Polyphthalamide (PPA)  (Unverified Data**)

Category Polymer , Thermoplastic , Polyphthalamide (PPA) , Polyphthalamide (PPA), 50% Glass Fiber Reinforced
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Zytel® HTN 52G45HSL BK083 Polyphthalamide (PPA)  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Zytel® HTN52G45HSL BK083 is a 45% glass reinforced, heat stabilized, lubricated high performance polyamide resin that can be molded in water heated molds. It is also a PPA resin.Information provided by DuPont Performance Polymers
Mechanical Properties Metric English Comments
Tensile Strength at Break 235 MPa

@Temperature 23.0 °C
34100 psi

@Temperature 73.4 °F
DAM; ISO 527
Elongation at Break 2.0 %

@Temperature 23.0 °C
2.0 %

@Temperature 73.4 °F
DAM; ISO 527
Flexural Modulus 15.5 GPa

@Temperature 23.0 °C
2250 ksi

@Temperature 73.4 °F
DAM; ISO 178
Charpy Impact Unnotched 6.50 J/cm²

@Temperature 23.0 °C
30.9 ft-lb/in²

@Temperature 73.4 °F
DAM; ISO 179/1eU
Charpy Impact, Notched 1.20 J/cm²

@Temperature 23.0 °C
5.71 ft-lb/in²

@Temperature 73.4 °F
DAM; ISO 179/1eA
Processing Properties Metric English Comments
Melt Temperature 320 - 330 °C
608 - 626 °F
DAM
Mold Temperature 85.0 - 105 °C
185 - 221 °F
DAM
Drying Temperature 100 °C
212 °F
DAM
Dry Time 6.00 - 8.00 hour
6.00 - 8.00 hour
DAM
Moisture Content <= 0.10 %
<= 0.10 %
DAM
Descriptive Properties Value Comments
Appearance Black Color
DAM
Forms Pellets
DAM
Generic Polyphthalamide (PPA)
DAM
Material Status Preliminary Data
DAM
Part Marking Code >PA6T/66-GF45<
ISO 11469; DAM
>PPA-GF45<
SAE J1344; DAM
Processing Method Injection Molding
DAM
Product Category Glass Reinforced Resins
DAM
Region Available - Global Yes
DAM
Resin Identification PA6T/66-GF45
ISO 1043; DAM
RoHS Compliance Contact Manufacturer
DAM