Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Performance Polymers Zytel® HTN FE350038 BK083 Polyphthalamide (PPA)  (Unverified Data**)

Category Polymer , Thermoplastic , Polyphthalamide (PPA) , Polyphthalamide (PPA), 30% Glass Fiber Reinforced
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Zytel® HTN FE350038 BK083 Polyphthalamide (PPA)  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Zytel® HTNFE350038 BK083 is a 33% glass reinforced, heat stabilized, lubricated, hydrolysis resistant high performance polyamide resin, developed for improved structural performance. It is also a PPA resin.Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.42 g/cc
0.0513 lb/in³
DAM; ISO 1183
Filler Content 33 %
33 %
DAM
Mechanical Properties Metric English Comments
Tensile Strength at Break 200 MPa

@Temperature 23.0 °C
29000 psi

@Temperature 73.4 °F
DAM; ISO 527
Elongation at Break 2.9 %

@Temperature 23.0 °C
2.9 %

@Temperature 73.4 °F
DAM; ISO 527
Tensile Modulus 10.2 GPa

@Temperature 23.0 °C
1480 ksi

@Temperature 73.4 °F
DAM; ISO 527
Flexural Strength 280 MPa

@Temperature 23.0 °C
40600 psi

@Temperature 73.4 °F
DAM; ISO 178
Flexural Modulus 9.40 GPa

@Temperature 23.0 °C
1360 ksi

@Temperature 73.4 °F
DAM; ISO 178
Fatigue Strength 53.2 MPa

@# of Cycles 173861 ,
Temperature 100 °C
7720 psi

@# of Cycles 173861 ,
Temperature 212 °F
DAM; 5Hz,R=0.1; 4mm; ISO 13003
66.5 MPa

@# of Cycles 30199 ,
Temperature 100 °C
9650 psi

@# of Cycles 30199 ,
Temperature 212 °F
DAM; 5Hz,R=0.1; 4mm; ISO 13003
79.8 MPa

@# of Cycles 10719 ,
Temperature 100 °C
11600 psi

@# of Cycles 10719 ,
Temperature 212 °F
DAM; 5Hz,R=0.1; 4mm; ISO 13003
93.1 MPa

@# of Cycles 3421 ,
Temperature 100 °C
13500 psi

@# of Cycles 3421 ,
Temperature 212 °F
DAM; 5Hz,R=0.1; 4mm; ISO 13003
106.4 MPa

@# of Cycles 1266 ,
Temperature 100 °C
15430 psi

@# of Cycles 1266 ,
Temperature 212 °F
DAM; 5Hz,R=0.1; 4mm; ISO 13003
119.7 MPa

@# of Cycles 442 ,
Temperature 100 °C
17360 psi

@# of Cycles 442 ,
Temperature 212 °F
DAM; 5Hz,R=0.1; 4mm; ISO 13003
Charpy Impact Unnotched 6.50 J/cm²

@Temperature 23.0 °C
30.9 ft-lb/in²

@Temperature 73.4 °F
DAM; ISO 179/1eU
Charpy Impact, Notched 1.00 J/cm²

@Temperature -40.0 °C
4.76 ft-lb/in²

@Temperature -40.0 °F
DAM; ISO 179/1eA
1.00 J/cm²

@Temperature 23.0 °C
4.76 ft-lb/in²

@Temperature 73.4 °F
DAM; ISO 179/1eA
Processing Properties Metric English Comments
Melt Temperature 325 °C
617 °F
DAM; Optimum
320 - 330 °C
608 - 626 °F
DAM
Mold Temperature 150 °C
302 °F
DAM; optimum
140 - 160 °C
284 - 320 °F
DAM
Drying Temperature 100 °C
212 °F
DAM
Dry Time 6.00 - 8.00 hour
6.00 - 8.00 hour
DAM
Moisture Content <= 0.10 %
<= 0.10 %
DAM
Descriptive Properties Value Comments
Appearance Black Color
DAM
Filler Glass Reinforced
DAM
Forms Pellets
DAM
Generic Polyphthalamide (PPA)
DAM
Material Status Preliminary Data
DAM
Part Marking Code >PA6T/XT-GF33<
ISO 11469; DAM
>PPA-GF33<
SAE J1344; DAM
Polymer Family High performance polyamide
DAM
Polymer Type Partially Aromatic PA, PPA
DAM
Processing Method Injection Molding
DAM
Product Category Glass Reinforced Resins
DAM
Hydrolysis Resistant Resins
DAM
Region Available - Global Yes
DAM
Resin Identification PA6T/XT-GF33
ISO 1043; DAM
RoHS Compliance Contact Manufacturer
DAM