Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Performance Polymers Zytel® HTN FE350038 BK083 Polyphthalamide (PPA)

Category Polymer , Thermoplastic , Polyphthalamide (PPA) , Polyphthalamide (PPA), 30% Glass Fiber Reinforced
Manufacturer DuPont Performance Polymers
Trade Name Zytel® HTN
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Zytel® HTN FE350038 BK083 Polyphthalamide (PPA).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
33% Glass Reinforced PPA High Performance Polyamide Zytel HTNFE350038 BK083 is a 33% glass reinforced heat stabilized lubricated hydrolysis resistant high performance polyamide resin developed for improved structural performance. It is also a PPA resinInformation provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.42 g/cc
0.0513 lb/in³
DAM; ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 200 MPa
29000 psi
DAM; ISO 527-1/-2
Elongation at Break 2.9 %
2.9 %
DAM; ISO 527-1/-2
Tensile Modulus 10.2 GPa
1480 ksi
DAM; ISO 527-1/-2
Flexural Strength 280 MPa
40600 psi
DAM; ISO 178
Flexural Modulus 9.40 GPa
1360 ksi
DAM; ISO 178
Charpy Impact Unnotched 6.50 J/cm²
30.9 ft-lb/in²
DAM; ISO 179/1eU
Charpy Impact, Notched 1.00 J/cm²
4.76 ft-lb/in²
DAM; ISO 179/1eA
1.00 J/cm²

@Temperature -40.0 °C
4.76 ft-lb/in²

@Temperature -40.0 °F
DAM; ISO 179/1eA
Descriptive Properties Value Comments
Additives Lubricants
Release agent
Delivery Form Pellets
Part Marking Code >PA6T/XT-GF33<
ISO 11469
>PPA-GF33<
SAE J1344
Processing Injection Moulding
Regional Availability Asia Pacific
Europe
Global
Near East/Africa
North America
South and Central America
Special Characteristics Heat stabilised or stable to heat