DuPont Performance Polymers Zytel® HTN FE8200 BK431 Polyphthalamide (PPA)  (Unverified Data**)

Category Polymer , Thermoplastic , Polyphthalamide (PPA)
Manufacturer DuPont Performance Polymers
Trade Name Zytel® HTN
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Zytel® HTN FE8200 BK431 Polyphthalamide (PPA)  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Unreinforced Toughened PPA High Performance Polyamide Zytel HTNFE8200 BK431 is an unreinforced toughened heat stabilized lubricated high performance polyamide resin for injection molding. It is also a PPA resin.Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
DAM; ISO 1183
Linear Mold Shrinkage, Flow 0.010 cm/cm
0.010 in/in
DAM; ISO 294-4 2577
Linear Mold Shrinkage, Transverse 0.010 cm/cm
0.010 in/in
DAM; ISO 294-4 2577
Mechanical Properties Metric English Comments
Tensile Strength, Yield 69.0 MPa
10000 psi
DAM; ISO 527-1/-2
Elongation at Break 14 %
14 %
DAM; Nominal; ISO 527-1/-2
Elongation at Yield 5.5 %
5.5 %
DAM; ISO 527-1/-2
Tensile Modulus 2.15 GPa
312 ksi
DAM; ISO 527-1/-2
Flexural Modulus 2.07 GPa
300 ksi
DAM; ISO 178
Charpy Impact, Notched 8.00 J/cm²
38.1 ft-lb/in²
DAM; ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 300 °C
572 °F
DAM; first heat; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 125 °C
257 °F
DAM; ISO 75-1/-2
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
DAM; IEC 60093
Descriptive Properties Value Comments
Part Marking Code >PA6T/XT-I<
ISO 11469
>PPA-I<
SAE J1344
Processing Injection Moulding
Regional Availability Asia Pacific
Europe
Global
Near East/Africa
North America
South and Central America
Special Characteristics Heat stabilised or stable to heat
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved