Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Performance Polymers Zytel® HTN FG52G35HSL BK011 Polyphthalamide (PPA)  (Unverified Data**)

Category Polymer , Thermoplastic , Polyphthalamide (PPA) , Polyphthalamide (PPA), 40% Glass Fiber Reinforced
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Zytel® HTN FG52G35HSL BK011 Polyphthalamide (PPA)  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Zytel®® HTNFG52G35HSL BK011 is a 35% glass reinforced, lubricated, heat stabilized high performance polyamide resin, developed for consideration into applications for the food industry. It is also a PPA resin.Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.45 g/cc
0.0524 lb/in³
DAM; ISO 1183
Filler Content 35 %
35 %
DAM
Linear Mold Shrinkage, Flow 0.0020 cm/cm

@Thickness 2.00 mm
0.0020 in/in

@Thickness 0.0787 in
DAM; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0080 cm/cm

@Thickness 2.00 mm
0.0080 in/in

@Thickness 0.0787 in
DAM; ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 170 MPa

@Temperature 23.0 °C
24700 psi

@Temperature 73.4 °F
50%RH; ISO 527
180 MPa

@Temperature 23.0 °C
26100 psi

@Temperature 73.4 °F
DAM; ISO 527
Elongation at Break 1.8 %

@Temperature 23.0 °C
1.8 %

@Temperature 73.4 °F
DAM; ISO 527
2.2 %

@Temperature 23.0 °C
2.2 %

@Temperature 73.4 °F
50%RH; ISO 527
Tensile Modulus 11.4 GPa

@Temperature 23.0 °C
1650 ksi

@Temperature 73.4 °F
50%RH; ISO 527
11.7 GPa

@Temperature 23.0 °C
1700 ksi

@Temperature 73.4 °F
DAM; ISO 527
Charpy Impact Unnotched 3.80 J/cm²

@Temperature 23.0 °C
18.1 ft-lb/in²

@Temperature 73.4 °F
DAM; ISO 179/1eU
3.80 J/cm²

@Temperature 23.0 °C
18.1 ft-lb/in²

@Temperature 73.4 °F
50%RH; ISO 179/1eU
Charpy Impact, Notched 0.800 J/cm²

@Temperature 23.0 °C
3.81 ft-lb/in²

@Temperature 73.4 °F
50%RH; ISO 179/1eA
0.800 J/cm²

@Temperature 23.0 °C
3.81 ft-lb/in²

@Temperature 73.4 °F
DAM; ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 60.0 µm/m-°C

@Temperature 23.0 - 55.0 °C
33.3 µin/in-°F

@Temperature 73.4 - 131 °F
DAM; ISO 11359-1/-2
Melting Point 310 °C
590 °F
10°C/min, First Heat; DAM; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 285 °C
545 °F
DAM; ISO 75-1/-2
Oxygen Index 25 %
25 %
DAM; ISO 4589-1/-2
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm

@Temperature 23.0 °C
1.00e+15 ohm-cm

@Temperature 73.4 °F
DAM; IEC 60093
Surface Resistance 1.00e+15 ohm

@Temperature 23.0 °C
1.00e+15 ohm

@Temperature 73.4 °F
DAM; IEC 60093
Processing Properties Metric English Comments
Melt Temperature 325 °C
617 °F
DAM; Optimum
320 - 330 °C
608 - 626 °F
DAM
Mold Temperature 85.0 - 105 °C
185 - 221 °F
DAM
Drying Temperature 100 °C
212 °F
DAM
Dry Time 6.00 - 8.00 hour
6.00 - 8.00 hour
DAM
Moisture Content <= 0.10 %
<= 0.10 %
DAM
Descriptive Properties Value Comments
Appearance Black Color
DAM
Filler Glass Reinforced
DAM
Forms Pellets
DAM
Generic Polyphthalamide (PPA)
DAM
Material Status Preliminary Data
DAM
Part Marking Code >PA6T/66-GF35<
ISO 11469; DAM
>PPA-GF35<
SAE J1344; DAM
Processing Method Injection Molding
DAM
Product Category Food Contact Resins
DAM
Glass Reinforced Resins
DAM
Region Available - Global Yes
DAM
Resin Identification PA6T/66-GF35
ISO 1043; DAM
RoHS Compliance Contact Manufacturer
DAM
Uses Food Applications, Non-specific
DAM
Users viewing this material also viewed the following: