Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Performance Polymers Zytel® RS LC3030 NC010 Nylon 610  (Unverified Data**)

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Nylon , Nylon 610
Manufacturer DuPont Performance Polymers
Trade Name Zytel® RS
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Zytel® RS LC3030 NC010 Nylon 610  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Zytel® RS LC3030 NC010 is a renewable sourced polyamide 610 containing a minimum of 60% renewably sourced ingredient by weight. It is an unreinforced, low viscosity grade, developed for extrusion applications (filaments).Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
DAM; ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Yield 62.0 MPa

@Temperature 23.0 °C
8990 psi

@Temperature 73.4 °F
DAM; ISO 527
Tensile Modulus 2.25 GPa

@Temperature 23.0 °C
326 ksi

@Temperature 73.4 °F
DAM; ISO 527
Flexural Modulus 2.10 GPa

@Temperature 23.0 °C
305 ksi

@Temperature 73.4 °F
DAM; ISO 178
Izod Impact, Notched (ISO) 5.00 kJ/m²

@Temperature 23.0 °C
2.38 ft-lb/in²

@Temperature 73.4 °F
DAM; ISO 180/1A
Charpy Impact, Notched 0.450 J/cm²

@Temperature 23.0 °C
2.14 ft-lb/in²

@Temperature 73.4 °F
DAM; ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 225 °C
437 °F
10°C/min; DAM; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C
131 °F
DAM; ISO 75-1/-2
Processing Properties Metric English Comments
Melt Temperature 250 °C
482 °F
DAM; Optimum
230 - 290 °C
446 - 554 °F
DAM
Mold Temperature 70.0 °C
158 °F
DAM; optimum
50.0 - 90.0 °C
122 - 194 °F
DAM
Drying Temperature 80.0 °C
176 °F
DAM
Dry Time 2.00 - 4.00 hour
2.00 - 4.00 hour
DAM
Moisture Content 0.15 %
0.15 %
DAM
Descriptive Properties Value Comments
Appearance Natural Color
DAM
Drying Recommended Yes, if moisture content of resin exceeds recommended level
DAM
Features Chemical Resistance, Good
DAM
Dimensional Stability, Good
DAM
Moisture Absorption, Low
DAM
Renewable Resource Content
DAM
Forms Pellets
DAM
Generic PA610
DAM
Material Status Preliminary Data
DAM
Part Marking Code >PA610<
ISO 11469; DAM
Polymer Family Polyamide
DAM
Polymer Type PA610
DAM
Processing Method Injection Molding
DAM
Product Category Renewably Sourced Resins
DAM
Toughened Resins
DAM
Unreinforced Resins
DAM
Region Available - Global Yes
DAM
Resin Identification PA610
ISO 1043; DAM
RoHS Compliance Contact Manufacturer
DAM
Uses Automotive Applications
DAM
Consumer Applications
DAM
Industrial Applications
DAM