Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont™ Sclairfilm® LX-3 LLDPE Film, Laminating, 50.8 µm Thickness  (discontinued **)

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Film Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont™ Sclairfilm® LX-3 LLDPE Film, Laminating, 50.8 µm Thickness  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by DuPont Packaging Polymers.A linear low density polyethylene film with an outstanding combination of toughness and durability. LX has superior tensile strength, puncture strength, elongation and heat seal strength compared to other sealant films. LX is a high performance film ideal for lamination to other materials, such as nylon or polyester films. In converter combinations, LX is particularly suited for the vacuum packaging of processed meats, cheese, coffee, and frozen foods.
Physical Properties Metric English Comments
Density 0.918 g/cc
0.0332 lb/in³
Moisture Vapor Transmission 0.470 cc-mm/m²-24hr-atm
1.19 cc-mil/100 in²-24hr-atm
ASTM E96 Procedure E
Water Vapor Transmission 9.30 g/m²/day
0.599 g/100 in²/day
ASTM E96 Procedure E
Oxygen Transmission 193 cc-mm/m²-24hr-atm
490 cc-mil/100 in²-24hr-atm
or 3800 cc/m²-24hr-atm for the film. ASTM D3985
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 600 %
600 %
ASTM D882
Tensile Modulus 0.170 GPa
24.7 ksi
ASTM D882
Dart Drop Test 175 g
0.386 lb
Seal Strength 2000 g/25 mm
2000 g/in
Sentinel Sealer Test
Film Tensile Strength at Break, MD 41.0 MPa
5950 psi
ASTM D882
Optical Properties Metric English Comments
Haze 9.0 %
9.0 %
ASTM D1003
Gloss 90 %
90 %
20°; ASTM D2457