DuPont™ Surlyn® 7940 Ionomer Resin, Lithium

Category Polymer , Thermoplastic , Ionomer , Ionomer, Molded
Manufacturer DuPont
Trade Name Surlyn®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont™ Surlyn® 7940 Ionomer Resin, Lithium.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Surlyn® 7940 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with lithium ions. The amount of MAA and neutralization levels for this grade are optimized to deliver extra clarity and stiffness compared with other grades of Surlyn®. The resin can be injection or blow molded, and is processable by extrusion into sheets or shapes.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 0.940 g/cc
0.0340 lb/in³
ASTM D792
Melt Flow 2.6 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.6 g/10 min

@Load 4.76 lb,
Temperature 374 °F
condition E; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 68
68
ASTM D2240
Tensile Strength, Ultimate 26.2 MPa
3800 psi
ASTM D638
Tensile Strength, Yield 15.2 MPa
2200 psi
50 mm/min cross speed; ASTM D638
Elongation at Break 285 %
285 %
ASTM D638
Flexural Modulus 0.420 GPa
60.9 ksi
ASTM D790
Izod Impact, Notched NB
NB
ASTM D256
Tensile Impact Strength 460 kJ/m²
219 ft-lb/in²
ASTM D1822S
Thermal Properties Metric English Comments
Melting Point 91.0 °C
196 °F
DSC
Deflection Temperature at 0.46 MPa (66 psi) 46.0 °C
115 °F
ASTM D648
Vicat Softening Point 63.0 °C
145 °F
Rate B, ASTM D1525-70
Optical Properties Metric English Comments
Haze 4.0 %

@Thickness 6.40 mm
4.0 %

@Thickness 0.252 in
ASTM D1003A