Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont™ Surlyn® 8140 Ionomer Resin, Sodium

Category Polymer , Thermoplastic , Ionomer , Ionomer, Molded
Manufacturer DuPont
Trade Name Surlyn®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont™ Surlyn® 8140 Ionomer Resin, Sodium.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Surlyn® 8140 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neutralization levels for this grade are optimized to deliver higher hardness and stiffness compared with other sodium ionomer grades of Surlyn®. The resin is ideal where high stiffness, high clarity and good abrasion resistance are desired. In golf ball covers, the resin provides good cut resistance, impact durability, high resilience and increased coefficient of restitution, particularly when used in blends with other cations. The resin is normally injection molded.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 0.960 g/cc
0.0347 lb/in³
ASTM D792
Melt Flow 2.6 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.6 g/10 min

@Load 4.76 lb,
Temperature 374 °F
condition E; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
ASTM D2240
Tensile Strength, Ultimate 37.0 MPa
5370 psi
ASTM D638
Tensile Strength, Yield 20.0 MPa
2900 psi
50 mm/min cross speed; ASTM D638
Elongation at Break 325 %
325 %
ASTM D638
Flexural Modulus 0.490 GPa
71.1 ksi
ASTM D790
Abrasion 426
426
NBS Index; ASTM D1630
Thermal Properties Metric English Comments
Melting Point 87.0 °C
189 °F
DSC
Vicat Softening Point 58.0 °C
136 °F
Rate B, ASTM D1525-70
Users viewing this material also viewed the following: