DuPont™ Surlyn® 8670 Ionomer Resin, Sodium  (discontinued **)

Category Polymer , Thermoplastic , Ionomer , Ionomer, Molded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont™ Surlyn® 8670 Ionomer Resin, Sodium  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Surlyn® 8670 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neutralization levels for this grade are optimized for ease of cryogenic grinding and optimum flow properties as a powder coating for glass. The resin also can be injection molded.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 0.940 g/cc
0.0340 lb/in³
ASTM D792
Melt Flow 20 g/10 min

@Load 2.16 kg,
Temperature 190 °C
20 g/10 min

@Load 4.76 lb,
Temperature 374 °F
condition E; ASTM D1238
Mechanical Properties Metric English Comments
Elongation at Break 494 %
494 %
ASTM D638
Flexural Modulus 0.159 GPa
23.1 ksi
ASTM D790
Izod Impact, Notched 4.80 J/cm
8.99 ft-lb/in
ASTM D256
Abrasion 170
170
NBS Index; ASTM D1630
Thermal Properties Metric English Comments
Melting Point 100 °C
212 °F
DSC
Deflection Temperature at 0.46 MPa (66 psi) 34.0 °C
93.2 °F
ASTM D648
Vicat Softening Point 71.0 °C
160 °F
Rate B, ASTM D1525-70