Material Notes:
Surlyn® 9720 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutralization levels for this grade are optimized to deliver low temperature toughness, plus abrasion resistance and stiffness. For wire and cable applications, this grade contains an antioxidant and meets Mil Spec P46124 MR, Type V, Class I requirements. The resin can be injection or blow molded, and is processable by extrusion into sheets or shapes.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 0.960 g/cc
0.0347 lb/in³
ASTM D792
Melt Flow 1.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
condition E; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 61
61
ASTM D2240
Tensile Strength, Ultimate 30.3 MPa
4390 psi
ASTM D638
Tensile Strength, Yield 11.7 MPa
1700 psi
50 mm/min cross speed; ASTM D638
Elongation at Break 440 %
440 %
ASTM D638
Flexural Modulus 0.250 GPa
36.3 ksi
ASTM D790
Izod Impact, Notched NB
NB
ASTM D256
Tensile Impact Strength 1260 kJ/m²
600 ft-lb/in²
ASTM D1822S
Tear Strength 102 kN/m
582 pli
Die C; ASTM D624
Abrasion 410
410
NBS Index; ASTM D1630
Thermal Properties Metric English Comments
CTE, linear 160 µm/m-°C

@Temperature -20.0 - 32.0 °C
88.9 µin/in-°F

@Temperature -4.00 - 89.6 °F
ASTM D696
Thermal Conductivity 0.250 W/m-K
1.74 BTU-in/hr-ft²-°F
Melting Point 92.0 °C
198 °F
DTA
Deflection Temperature at 0.46 MPa (66 psi) 43.0 °C
109 °F
ASTM D648
Vicat Softening Point 71.0 °C
160 °F
Rate B, ASTM D1525-70
Brittleness Temperature -110 °C
-166 °F
ASTM D746
Flame Spread 25.4 mm/min
1.00 in/min
ASTM D635
Optical Properties Metric English Comments
Haze 12 %

@Thickness 6.35 mm
12 %

@Thickness 0.250 in
ASTM D1003A
Gloss 25 %
25 %
20° per ASTM D523-6