DuPont Surlyn® SURSG201UG  (discontinued **)

Category Polymer , Thermoplastic , Ethylene Methyl Acrylate
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Surlyn® SURSG201UG  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Surlyn Reflections® SG201UG is a modified ionomer resin for applications that require a high gloss, molded in color surface finish directly from the mold. The material is weatherable, durable and provides improved scratch and abrasion resistance. Surlyn Reflections® SG201UG is an excellent, lower cost, more environmentally friendly alternative to painting.Information provided by DuPont™
Physical Properties Metric English Comments
Density 1.043 g/cc
0.03768 lb/in³
ASTM D792-ISO 1183
Linear Mold Shrinkage 0.010 cm/cm
0.010 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 44.8 MPa
6500 psi
ASTM D638 ISO 527-2
Elongation at Break >= 200 %
>= 200 %
ASTM D638 ISO 527-2
Flexural Modulus 1.00 GPa
145 ksi
ASTM D790
Izod Impact, Notched 2.67 J/cm
5.00 ft-lb/in
Low Temp; ASTM D256
6.41 J/cm
12.0 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 93.6 µm/m-°C

@Temperature 20.0 °C
52.0 µin/in-°F

@Temperature 68.0 °F
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 58.0 °C
136 °F
ASTM D648
Vicat Softening Point 190 °C
374 °F
ASTM D1525, ISO 306