Material Notes:
Melinex® 306 is a clear, smooth pretreated polyester film. Melinex® 306 is produced from a lightly filled polymer, giving it a very smooth surface. The two side chemical coating provides adhesion to magnetic oxides and a variety of inks, but also combines some antistatic properties to reduce the amount of static charge buildup that results from roll processing (winding and unwinding). This anticharge property helps reduce debris and contaminant attraction resulting in a cleaner film process for our customers.Also available in 286 GaugeInformation provided by DuPont.
Physical Properties Metric English Comments
Density 1.395 g/cc
0.05040 lb/in³
ASTM D1505
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 95.8 MPa

@Strain >=5.00 %
13900 psi

@Strain >=5.00 %
ASTM D882A
Film Elongation at Break, MD 117 %
117 %
ASTM D882A
Film Tensile Strength at Break, MD 191 MPa
27700 psi
ASTM D882A
Film Tensile Strength at Break, TD 225 MPa
32600 psi
ASTM D882A
Optical Properties Metric English Comments
Transmission, Visible 90.2 %

@Thickness 0.0762 mm
90.2 %

@Thickness 0.00300 in
TLT; ASTM D1003
Descriptive Properties Value Comments
Coefficient of Hygroscopic Expansion 7E-6/%RH
40-80% RH
Surface Roughness 0.008 microns