Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Teijin Films Melinex® 487 Polyester Film, 200 Gauge

Category Polymer , Film , Thermoplastic , Polyester, TP , Polyester Film
Manufacturer DuPont Teijin Films (DTF)
Trade Name Melinex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Teijin Films Melinex® 487 Polyester Film, 200 Gauge.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Melinex® 487 is a high-yield, white film that is coated on one side for adhesion to inks, coatings, laser printing, and thermal transfer printing.Information provided by DuPont.
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
ASTM D1505-79 (Mod. to DuPont method)
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 228 MPa
33000 psi
ASTM D882A
Film Tensile Strength at Yield, TD 228 MPa
33000 psi
ASTM D882A
Film Elongation at Break, MD 140 %
140 %
ASTM D882A
Film Elongation at Break, TD 100 %
100 %
ASTM D882A
Coefficient of Friction, Dynamic 0.40
0.40
[in<sup>2</sup>/lb], A-B; ASTM D1894
Film Tensile Strength at Break, MD 159 MPa
23000 psi
ASTM D882A
Film Tensile Strength at Break, TD 159 MPa
23000 psi
ASTM D882A
Thermal Properties Metric English Comments
Shrinkage, MD 2.5 %

@Temperature 190 °C,
Time 300 sec
2.5 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Optical Properties Metric English Comments
Transmission, Visible 33 %
33 %
TLT; ASTM D1003
Users viewing this material also viewed the following: